石油炼制与化工 ›› 2026, Vol. 57 ›› Issue (12): 34-41.

• 加工工艺 • 上一篇    下一篇

催化裂化装置滤渣回炼工艺问题分析与对策研究

李荣亚,杨志鹏,康浩,郑小辉,隋建国,李超,贾伟峰,曹阳   

  1. 浙江石油化工有限公司
  • 收稿日期:2026-06-22 修回日期:2026-08-04 出版日期:2026-12-12 发布日期:2026-11-17
  • 通讯作者: 杨志鹏 E-mail:zsh_yangzp@rong-sheng.com

ANALYSIS AND COUNTERMEASURES STUDY ON PROBLEUMS OF FILTER SLAG RECYCLE PROCESS IN CATALYTIC CRACKING UNITS

  • Received:2026-06-22 Revised:2026-08-04 Online:2026-12-12 Published:2026-11-17

摘要: 对催化裂化油浆脱固系统产生的滤渣进行回炼虽为资源综合利用的常见途径,但实际工业运行结果表明其对装置的长周期运行存在显著负面影响。以某炼油厂4.50 Mt/a重油催化裂化装置为对象,系统分析了几个滤渣回炼周期[回炼时间为24~207 d,回炼比(滤渣回炼量与催化裂化总进料量的质量比,下同)为0.57%~0.67%]的运行数据与检修结果。结果表明:滤渣回炼导致沉降器汽提段介质密度持续下降,回炼时间最长(207d)时上部介质密度降幅达14.37%,第四周期(回炼时间为134d,回炼比为0.67%)时降幅高达19.56%;脱前油浆灰分由正常值(0.20%~0.30%)升高至0.93%,远超设计值(0.6%);停工检修证实沉降器汽提段第1~第6层严重结焦,且原料换热器存在催化剂沉积。定量分析结果表明,滤渣中质量分数28%~32%的重组分在反应温度低于530℃时无法汽化,这些组分携同高含量催化剂细粉(质量分数为2.6%~8.5%)在沉降器内缩合生焦,是导致上述问题的根本原因。因此,建议滤渣不宜回催化裂化装置回炼,应统筹协调其他处理途径,研究结果可为同类装置滤渣处置决策提供参考。

关键词: 催化裂化, 滤渣, 回炼, 沉降器, 结焦, 油浆, 灰分, 催化剂沉积

Abstract: Although the recycling of filter residue generated by the catalytic cracking slurry desulfurization system is a common way for comprehensive resource utilization, actual industrial operation has shown that it has a significant negative impact on the long-term operation of the device. This article takes the 4.50 Mt/a heavy oil catalytic cracking unit of a certain refinery as the object, and systematically analyzes the operating data and maintenance results of several filter residue recycling cycles [recycling time of 24—207 d, recycling ratio (w, the same below) of 0.57%—0.67%].Research has found that the recycling of filter residue leads to a continuous decrease in the density of the settling and stripping sections. At the longest recycling time (207 d), the upper density decreased by 14.37%, and in the fourth cycle (134 d, recycling ratio 0.67%), the decrease was as high as 19.56%;the ash content of the pre stripping slurry increased from the normal range of 0.20%—0.30% to 0.93%, far exceeding the design value of 0.6%;shut down maintenance confirmed severe coking in the first to sixth layers of the stripping section,and catalyst deposition in the raw material heat exchanger.Quantitative analysis shows that the heavy components with a mass fraction of 28%—32% in the filter residue cannot vaporize when the reaction temperature is below 530 ℃. These components, along with high content catalyst fine powder (mass fraction of 2.6%—8.5%), coalesce into coke in the settler, which is the fundamental cause of the problem. The study suggests that the filter residue should not be recycled to the catalytic cracking unit for refining and other treatment methods should be coordinated.The results could provide reference for the disposal decisions of filter residue in similar units.

Key words: catalytic cracking, filter residue, recycling, settling device, coking, oil slurry, ash content, catalyst deposition