石油炼制与化工 ›› 2026, Vol. 57 ›› Issue (12): 42-50.

• 催化剂 • 上一篇    下一篇

热处理条件对NiW-柠檬酸/Al2O3催化剂原生积炭形成以及加氢脱氮和芳烃饱和性能的影响

朱进,翟维明,刘锋,熊瑞丰,闫亚文,李会峰   

  1. 中石化石油化工科学研究院有限公司 国家能源石油炼制技术研发(实验)中心
  • 收稿日期:2026-05-29 修回日期:2026-07-08 出版日期:2026-12-12 发布日期:2026-11-17
  • 通讯作者: 李会峰 E-mail:lihf.ripp@sinopec.com

EFFECT OF HEAT TREATMENT CONDITIONS ON THE FORMATION OF PROTOGENESIS CARBON DEPOSITS, HYDRODENITROGENATION, AND AROMATICS SATURATION PERFORMANCE OF NiW-CITRIC ACID/Al2O3 CATALYST

  • Received:2026-05-29 Revised:2026-07-08 Online:2026-12-12 Published:2026-11-17

摘要: 为了探究热处理条件对NiW-柠檬酸/Al2O3催化剂原生积炭形成以及咔唑加氢脱氮和1-甲基萘芳烃饱和性能的影响,借助激光拉曼光谱、碳含量分析、程序升温氧化、透射电子显微镜和X射线光电子能谱等对相应氧化态和硫化态样品进行表征。结果表明:干燥样品中的柠檬酸可起到减弱金属与载体相互作用以及隔离金属物种的作用,经硫化后钨的硫化度和活性相Ni含量与总Ni含量之比(NiNi-W-S/Ni总比)最高;与干燥样品相比,焙烧样品(空气或氮气气氛)由于金属与载体相互作用增强,其钨硫化度和NiNi-W-S/Ni总比均有所降低;氮气中焙烧后柠檬酸发生热缩聚反应,部分转化成固体炭物种保留在催化剂上,且激光拉曼光谱上出现较明显的G峰,经硫化后催化剂总碳含量和“毗邻”活性相的碳含量均最高;不同条件热处理所得样品的活性相片晶平均长度没有明显变化,但平均堆叠层数有一定差异,其中氮气中焙烧样品的堆叠层数最低。对于咔唑加氢脱氮反应,干燥样品的活性最高,且未脱除氮的加氢产物占比最低。对于1-甲基萘加氢饱和反应,氮气中焙烧样品的活性最高,归因于其“毗邻”活性相的碳对活性相形貌结构的“修饰”作用。空气中焙烧样品的加氢脱氮和芳烃加氢饱和活性均处于干燥样品和氮气中焙烧样品之间。

关键词: NiW催化剂, 柠檬酸, 热处理, 原生积炭, 加氢脱氮, 芳烃饱和

Abstract: To investigate the effect of heat treatment conditions on the formation of protogenesis carbon deposits, as well as hydrodenitrogenation of carbazole and hydrogenation of 1-methylnaphthalene on NiW citric acid/Al2O3 catalyst, the corresponding oxidic and sulfided samples were characterized by laser raman spectroscopy, carbon content analysis, programmed temperature oxidation, transmission electron microscopy, and X-ray photoelectron spectroscopy. The results showed that the presence of citric acid in the dried sample can weaken the interaction between the metal and the support, as well as isolate metal species. After sulfidation, the sulfidation degree of tunsten and NiNi-W-S/Nitotal ratio of the dried sample were the highest. Compared with the dried sample, the sample calcined in air and the sample calcined in N2 have a decrease in sulfidation degree of tungsten and NiNi-W-S/Nitotal ratio due to the enhanced interaction between the metal and the support. The sample calcined in N2 undergoes thermal condensation reaction due to the presence of citric acid, and some of it is converted into carbon deposits on the catalyst; moreover, a distinct G peak appears in the laser raman spectroscopy; after sulfidation, the contents of its total carbon and the carbon in the vicinity of active phase are both the highest. The average length of active phase of the samples obtained under different heat treatment conditions did not show significant changes, but there were some differences in the average stacking number, with the sample calcined in N2 having the lowest. For hydrodenitrogenation of carbazole, the activity of the dried sample is the highest, and the proportion of partly-hydrogenated products with N heteroatom is also the lowest. For hydrogenation of 1-methylnaphthalene, the sample calcined in nitrogen has the highest activity, attributed to the modification effect of protogenesis carbon deposits in the vicinity of the active phase on the morphology and structure of the active phase. The hydrodenitrogenation and aromatic saturation activities of the sample calcined in air are both between those of the sample dried in air and the sample calcined in N2.

Key words: NiW catalyst, citric acid, heat treatment, protogenesis carbon deposit, hydrodenitrogenation, aromatics saturation