摘要: 以NaY分子筛为原料,采用后处理工艺制备出能够基本达到工业要求的催化剂,并采用XRD、BET、NH3-TPD、IR、SEM等方法对催化剂进行物化性质表征。结果表明,与常规方法制备的对比剂相比,后处理方法制备催化剂的表面有许多凹陷的大孔结构,一定量的稀土离子从超笼迁移到方钠石笼,且方钠石笼中容纳了更多的稀土离子,催化剂比表面积和孔体积大,酸性强,重油转化率高,微反活性高。
Abstract: A FCC catalyst prepared by post-processing technology using NaY molecular sieve as a raw material was characterized by XRD, BET, NH3 TPD, IR and SEM techniques. The results show that compared with a reference catalyst treated by conventional method, the catalyst post-processed has many sunken macroporous structure on the surface, a certain amount of rare earth ions from supercage migrates to sodalite cage, and more rare earth ions exists in the sodalite cage than in the reference catalyst. The post-treated catalyst has a larger surface area and pore volume, stronger acidity, higher heavy oil conversion rate, and micro reaction activity.
王世环 张杰潇 许明德 田辉平. FCC催化剂后处理工艺制备催化剂的表征[J]. 石油炼制与化工, 2014, 45(8): 11-16.
0 / / 推荐
导出引用管理器 EndNote|Ris|BibTeX
链接本文: http://www.sylzyhg.com/CN/
http://www.sylzyhg.com/CN/Y2014/V45/I8/11