石油炼制与化工 ›› 2015, Vol. 46 ›› Issue (6): 89-94.

• 设备及防腐 • 上一篇    下一篇

常压塔塔顶循环结垢腐蚀的原因分析及解决措施

崔蕊,于焕良,钟广文,王云强   

  1. 中石化股份天津分公司研究院
  • 收稿日期:2014-09-18 修回日期:2014-12-03 出版日期:2015-06-12 发布日期:2015-05-26
  • 通讯作者: 崔蕊 E-mail:cr729@126.com

CAUSES OF FOULING AT TOP CIRCULATION OF ATMOSPHERIC COLUMN AND COUNTERMEASURES

  • Received:2014-09-18 Revised:2014-12-03 Online:2015-06-12 Published:2015-05-26

摘要: 针对天津石化公司3号常减压蒸馏装置常压塔塔顶循环管线结垢的问题,详细分析了垢物组成,并从结垢机理和塔顶各物料的性质分析了造成常压塔塔顶循环管线结垢的原因。通过减少缓蚀剂注入量,减少有机胺的注入量,调整常压塔塔顶注水方案,添加阻垢分散剂等措施,装置塔顶循环量达到设计值,且对下游产品未造成影响,解决了常减压蒸馏装置常压塔顶循环管线结垢问题。

Abstract: To study the fouling causes of atmospheric column in Tianjin petrochemical company, the composition of the scaling and the properties of materials at the top of atmospheric column were analyzed. Based on the analysis results, technical measures were suggested,such as changing amount of corrosion inhibitor and regulating solution of injection water, adopting the new process and scale dispersant, resulting in improved fouling situation of the atmospheric column. The circulation volume at the top of column meets the design value and no harmful effect is found in down-stream products.